[1]江 勇,王春輝,李鵬沖.特殊扣鋼管的疲勞理論、試驗與應用[J].焊管,2017,40(10):1-14.[doi:10.19291/j.cnki.1001-3938.2017.10.001]
 JIANG Yong,WANG Chunhui,Li Pengchong.Fatigue Theory,Tests and Application of Premium Thread Steel Pipes[J].,2017,40(10):1-14.[doi:10.19291/j.cnki.1001-3938.2017.10.001]
點擊復制

特殊扣鋼管的疲勞理論、試驗與應用()
分享到:

《焊管》[ISSN:1001-3938/CN:61-1160/TE]

卷:
40
期數:
2017年第10期
頁碼:
1-14
欄目:
行業綜述
出版日期:
2017-10-28

文章信息/Info

Title:
Fatigue Theory,Tests and Application of Premium Thread Steel Pipes
文章編號:
10.19291/j.cnki.1001-3938.2017.10.001
作者:
江 勇王春輝李鵬沖
 中油管道物資裝備有限公司, 河北 廊坊 065000
Author(s):
JIANG Yong WANG Chunhui Li Pengchong
 China Petroleum Pipeline Material and Equipment Co., Ltd., Langfang 065000, Hebei, China
關鍵詞:
特殊扣鋼管疲勞應力集中LET S-N曲線
Keywords:
premium thread steel pipe fatigue stress concentration LET S-N curve
分類號:
TE931.2
DOI:
10.19291/j.cnki.1001-3938.2017.10.001
文獻標志碼:
A
摘要:
為了促進特殊扣鋼管抗疲勞性能的進一步提升,從特殊扣鋼管管體材料的疲勞、螺紋連接的疲勞、螺紋連接的設計等方面進行了研究。分析了循環載荷作用下特殊扣鋼管疲勞產生的主要原因;以法國V&M公司和阿根廷Tenaris公司等國外主流抗疲勞特殊扣產品為例,闡述了螺紋設計時摩擦系數、螺距、錐度和應力釋放結構對疲勞的影響;介紹了研究特殊扣鋼管疲勞問題的試驗裝置及測取S-N曲線的基本問題,重點講述了共振型全尺寸疲勞評價試驗裝置的試驗原理。研究結果表明,影響螺紋結構套管疲勞強度的最主要因素是應力集中系數(SCF),螺紋結構往往在公端最后一圈螺紋LET處應力最大,應力集中系數也較大。因此,螺紋結構套管在結構設計上應盡量采用圓滑過渡來降低應力集中系數,母端外側應考慮抗彎曲機構;可適當降低母端的壁厚、提高螺紋結構的加工精度,在設計上盡量考慮應力釋放部分及去除殘余應力工藝的使用,從而提高特殊扣鋼管的抗疲勞性能。
Abstract:
In order to promote the further improvement of the anti-fatigue performance of premium thread steel pipe,in this article,the fatigue performance of pipe body material was researched,as well as the fatigue and design of threaded connections. The main reason of fatigue of premium thread steel pipe was analyzed. Take anti-fatigue premium thread products of French V&M company and Argentine Tenaris company for instance,the influence of frictional coefficient,pitch, taper and stress releasing structure on fatigue at design time were expounded,the basic issues of fatigue test machine and S-N curve measure were introduced,and the test principles of resonance full-scale test apparatus of fatigue evaluation were focused on. According to the research results,the major factor influencing thread casing fatigue strength was stress concentration factor(SCF) which had a larger value in LET of pin with the maximum stress. Therefore,smooth transition was used to reduce SCF in thread casing structure design,resistance to deflection structure should be considered outside female ends;wall thickness of female ends should be reduced,machining accuracy of thread structure should be improved,stress releasing and residual stress removal should be used to improve the fatigue performance of premium connection of steel pipe.

參考文獻/References:

[1] BERTINI L,SANTUS C,BOULET J,et al. Resonant Bench for Fatigue Testing of Steel Drill Pipe Connections[J]. A-IAS,2012.
[2] LIU H B,ZHAO X L. Fatigue of Subsea Pipelines under Combined Actions[C]//Proceedings of the Twenty-third(2013) International Offshore and Polar Engineering. Anchorage,Alaska,USA:[s.n.]. 2013:147-154.
[3] JORDAN G R,MERLIAHMAD M,GRITTINI S,et al.Fatigue analysis of OCTG premium connections:Theory,laboratory testing and application[C] //Offshore Technology Conference-Asia. 2014:1173-1187.
[4] WITTENBERGHE J V,BAETS P D,WAELE W D,et al. Numerical and experimental study of the fatigue of threaded pipe couplings[C]//Contact/surface,2009:163-174.
[5] WITTENBERGHE J V,PAUW J D,BAETS P D,et al. Experimental determination of the fatigue life of modified threaded pipe couplings[J]. Procedia Engineering,2010,2(1):1849-1858.
[6] BRAUN M. FATIGUE. Assessment of Threaded Riser Connections[D]. Norwegian University of Science and Technology,2014.
[7] JACKY M,SHILLING R B,PAYNE M,et al. Higeaded and Coupled Connectors for Dynamic Riser Application[J]. SPE 108708,2007:1-11.
[8] WITTENBERGHE J V,GALLE T,WAELE W D,et al. Experimental analysis of the fatigue life of threaded pipe connections under cyclic bending[C]//Sustainable Construction and Design(SCAD-2012). Ghent University,Laboratory Soete,2012:89-97.
[9] MEERTENS B,BAETS P D,WAELE W D,et al. Fatigue behaviour of threaded couplings-experimental research[J]. Occupational Therapy International,2010,22(1):19-27.
[10] WITTENBERGHE J V,BAETS D P,WAELE W D,et al. Design Characteristics that Improve the Fatigue Life of Threaded Pipe Connections [J]. Sustainable Construction & Design,2011, 2(2):334-341.
[11] DNV-RP-C203:2011,Recommended Practice C203-Fatigue Design of Offshore Steel Structures[S].
[12] BS 7608—1999,Code of Practice for Fatigue Design and Assessment of Steel Structures[S].
[13] API RP 7G:1998,Recommended Practice for Drill Stem Design and Operating Limits[S].
[14] API Specification 7:1998,Specification for Rotary Drill Stem Elements[S].
[15] TEODORIU C,FALCONE G. Fatigue Life Prediction of a Butress Casing Connection Exposed to Large Temperature Variations[C]//Stanford Workshop on Geothermal Reservoir Engineering,2008.
[16] GALLE T,WAELE D,BAETS P D,et al. Influence of Design Features on the Structural Integrity of Threaded Pipe Connections[J] . Sustainable Construction & Design, 2011,
2(2):237-245.
[17] HAN S,KNIGHT M,BRENNAN F P. Fatigue Analysis of Drillstring Threaded Connections[C]//Proceedings of The Thirteenth(2003) International Offshore and Polar Engineering Conference,2003:202-208.
[18] KRISYOFFERSEN B. Improvement Fatigue Performance of  Threaded Drillstring Connections by Cold Rolling[D]. Fakultet for Ingeniфrvitenskap Og Teknologi,2002.
[19] SEAN E E,TOM H. Improved Rotary-Slip dies help boost drillstring life[J]. Drilling Contractor,2000(1):30-31.
[20] DARCIS P P,MARINESGARCIA I,MARQUES E C,et al. Fatigue Performance of Machined Pipe Outer Surface[C]//Proceedings of the Nineteenth(2009) International Offshore and Polar Engineering Conference. 2009:534-540.
[21] SANTI N J,CARCAGNO G E,TOSCANO R. Premium and Semi-Premium Connections Design Optimization for Varied Drilling-With-Casing Applications[C]//Offshore Technology Conference,2005:1-10.
[22] XU H L,SHIT H,ZHANG Z,et al. Loading and Contact Stress Analysis on the Thread Teeth in Tubing and Casing Premium Threaded Connection[J]. Mathematical Problems in Engineering,2014(1):1-11.
[23] 呂英民,陳海量,仇偉德,等. 材料力學[M]. 東營:中國石油大學出版社,2007.
[24] BODINE A G. Sonic well pump tubing string:United States Patent,US2992613[P]. 1961.
[25] SCHREIER K,JONCTION F. Notamment pour tige de forageFrench Patent:French patent,FR1317815[P]. 1963.
[26] DELANGE R W,EVANS M E. Threaded and coupled connection for improved fatigue resistance:United States Patent,US 6609735 B1[P]. 2003.
[27] VERDILLON L. Fatigue-resistant threaded bevelledtubular element:United States Patent,US 6752436 B1[P]. 2004.
[28] WITTENBERGHE J V,PAUW J D. Fatigue investigation of threaded pipe connections[J]. Sustainable Construction & Design,2010,1(1):182-189.
[29] CELLINE S,OLIVIER C,ANTOINE D. OTC-22442-MS:Development And Validation With Testing Of A High Strength Steel Fatigue Resistant Threaded & Coupled premium Connectors Product Line For Outer Production Riser And Single Barrier Riser Applications in Deepwater And Ultra Deepwater[C]//Offshore Technology Conference,2011:1-19.
[30] SHIELD J,WIGHTMAN J,PAPPAS J,et al. OTC-24069:Fatigue Testing of Shrink-Fit Couplings for Joining High Strength Steel Riser Pipe[C]//Offshore Technology Conference,2013:1-14.
[31] ASSANELLI A P,XU Q,BENEDETTO F,et al. Numerical/Experimental Analysis of an API 8Round Connection[J]. Journal of Energy Resources Technology,1997,119(2):81-88.
[32] YAMAMOTO K I,KOBAYASHI K,MAGUCHI T,et al. Stress analysis of premium threaded connection FOX by finite element method[J]. Kawasaki Steel Technical Report,1990(22):41-47.
[33] JFE Steel Corporation. FOX Premium Threaded Connection[EB/OL]. [2017-03-22]. http://www.docin.com/p-543339042.html
[34] SUGINO M,NAKAMURA K,YAMAGUCJI S,et al. Development of an innovative high-performance premium threaded connection for OCTG[C]//Offshore Technology Conference. Houston,Texas,USA,OTC 20734. 2010.
[35] JELLISON M J,CHANDLER R B,MURADOV A,et al. New BHA connection enhances fatigue performance for difficult drilling applications[J]. Drilling Contractor,2006:18-20.
[36] Vallourec & Mannesmann. VAM book [EB/OL]. [2017-03-22]. http://www.vamservices.com/Library/files/VAM%C2%AE%20Book.pdf.
[37] TenarisHydril. Premium Connections Catalogue[EB/OL].[2017-03-22]. http://www.tenaris.com/en/ProductsPremium Connections.aspx.
[38] AGGARWAL R K,BHAT S U,MELING T S,et al. Qualification of Enhanced SCR Design Solutions For Improving Fatigue Life At Touch Down Zone[C]//Proceedings of the Sixteenth(2006) International Offshore and Polar Engineering Conference,2006:52-59.
[39] VEIDT M,BEREZOVSKI A. Design and Application of A Drill Pipe Fatigue Test Facility[C]//Proceedings of SIF2004 Structural integrity and fracture,2004:367-373.
[40] FANG X M,YAN Z C,WANG L Q,et al.Experiment and Finite Analysis on ResonantBendingFatigue of Marine Risers[J]. The OpenMechanical Engineering Journal,2015(9):205-212.
[41] REICHERT B,NGUYEN T,ROLOVIC R,et al. Advancements in Fatigue Testing and Analysis[C]//Proceedings of SPE/ICoTA Coiled Tubing and Well Intervention Conference and Exhibition,2016:1-11.
[42] FASZOLD J,ROSINE R,SPOERING R. Full-Scale Fatigue Testing With 130K Yield Tubing[J]. SPE 153945,2012.
[43] WITTENBERGHE J V. Experimental Analysis and Modelling of the Fatigue Behaviour of Threaded Pipe Connections[D]. Belgium:Ghent University,2011.

相似文獻/References:

[1]李春林.條形碼技術在鋼管企業中的應用[J].焊管,2007,30(4):47.[doi:1001-3938(2007)04-0047-02]
 LI Chun-lin.Application of Bar Code Technology by Steel Pipe Enterprise[J].,2007,30(10):47.[doi:1001-3938(2007)04-0047-02]
[2]張朝生 編譯.高強度管道鋼管表面應力腐蝕裂紋的研究[J].焊管,2007,30(4):82.[doi:1001-3938(2007)04-0083-03]
 Edited and Translated by ZHANG Chao-sheng.Study on Surface Stress Corrosion Crack of High Strength Pipeline[J].,2007,30(10):82.[doi:1001-3938(2007)04-0083-03]
[3]孫 宏.高鋼級螺旋縫焊接鋼管拉伸試樣類型選擇[J].焊管,2007,30(5):36.[doi:1001-3938(2007)05-0036-03]
 SUN Hong.Study of Choosing the Tensile Test Specimen’s Type for High Grade SSAW Steel Pipe[J].,2007,30(10):36.[doi:1001-3938(2007)05-0036-03]
[4]郭繼富,王素娟,張艷龍,等.鋼管數控仿形鋸鋸片TiAlN涂層技術的應用[J].焊管,2007,30(6):48.[doi:1001-3938(2007)06-0048-03]
 GUO Ji-fu,WANG Shu-juan,ZHANG Yan-long,et al.Application of TiAlN Coating Technology of Numerical Control and Profile Modeling Saw Chip for Steel Pipe[J].,2007,30(10):48.[doi:1001-3938(2007)06-0048-03]
[5]岳進才.常見鋼管質量問題及成因分析[J].焊管,2008,31(1):64.[doi:1001-3938(2008)01-0064-06]
 YUE Jin-cai.Common Quality Problem & Cause Analyses of Steel Pipe[J].,2008,31(10):64.[doi:1001-3938(2008)01-0064-06]
[6]趙 坤.淺談ERW鋼管錯邊缺陷[J].焊管,2008,31(2):67.[doi:1001-3938(2008)02-0067-02]
 ZHAO Kun.Brief Discussion on Offset Defect of ERW Pipe[J].,2008,31(10):67.[doi:1001-3938(2008)02-0067-02]
[7]郭艷玲,高真鳳,張興虎.俄羅斯國內鋼管產銷趨勢[J].焊管,2008,31(2):86.[doi:1001-3938(2008)02-0086-05]
 GUO Yan-ling,GAO Zhen-feng,ZHANG Xing-hu.Trends of Steel Pipe Production and Sale in Russia[J].,2008,31(10):86.[doi:1001-3938(2008)02-0086-05]
[8]張正龍.Φ219 mm鋼管內涂層“縮坑”缺陷分析[J].焊管,2008,31(4):64.[doi:1001-3938(2008)04-0064-03]
 ZHANG Zheng-long.Analysis on ‘Shrinkage Dent’of Φ219 mm Steel Pipe Internal Coating[J].,2008,31(10):64.[doi:1001-3938(2008)04-0064-03]
[9]馮來義,羅曉梅.鋼管預熱中頻設備可控硅的正確使用及保護[J].焊管,2008,31(5):66.[doi:1001-3938(2008)05-0066-04]
 FENG Lai-yi,LUO Xiao-mei.Corrective Using & Protecting of Silicon Controlled Rectifier in Intermediate Frequency Induction Heating Equipment[J].,2008,31(10):66.[doi:1001-3938(2008)05-0066-04]
[10]袁厚之.高鉻合金軋輥和矯直輥的研制及推廣[J].焊管,2009,32(3):31.[doi:1001-3938(2009)03-0031-04]
 YUAN Hou-zhi.Research and Extendtion of High Cr Alloy Roller and Straigthening Roller[J].,2009,32(10):31.[doi:1001-3938(2009)03-0031-04]

備注/Memo

備注/Memo:

收稿日期:2017-04-07

作者簡介:江  勇(1980—),男,湖北蘄春人,工程師,主要從事油井管采購和研究工作。